Hotline:0755-22277778
Tel:0755-22277778
Mobile:13826586185(Mr.Duan)
Fax:0755-22277776
E-mail:duanlian@xianjinyuan.cn
In the electronics industry, conductive silver paste is widely used due to its excellent conductivity and reliable bonding ability. The low-temperature conductive silver adhesive launched by Advanced Institute (Shenzhen) Technology Co., Ltd. has attracted high attention from the market due to its unique low-temperature curing characteristics and excellent conductivity. This article will delve into the impact of curing time onResearch Platinum Brand YB6016 Low Temperature Conductive Silver AdhesiveThe impact of conductivity.
The curing time is the time required to guide the transition of silver paste from liquid to solid state. For low-temperature conductive silver paste, the length of curing time directly affects its conductivity. Short or long curing time can have adverse effects on conductivity.
The curing time is too short
When the curing time is too short,Conductive silver adhesiveThe silver particles in the middle did not fully contact and connect, resulting in an incomplete conductive network. This will interrupt the conductive path, increase the resistance, and thus reduce the conductivity. In addition, a too short curing time may lead to stress concentration inside the silver paste, forming microcracks and further deteriorating the conductivity.
The curing time is too long
On the contrary, prolonged curing time can also have a negative impact on conductivity. Long term solidification can lead to excessive aggregation of silver particles, forming aggregates that hinder the uniform distribution of the conductive network. Meanwhile, excessively long curing time may cause excessive decomposition of organic components inside the silver paste, resulting in bubbles and voids, and reducing its conductivity.
In order to ensure the optimal conductivity of low-temperature conductive silver paste, it is necessary to determine its optimal curing time.Advanced Institute (Shenzhen) Technology Co., LtdThrough extensive experimental research, it has been found that the optimal curing time for YB6016 low-temperature conductive silver paste from Yanbo brand is usually between 30 minutes and 1 hour. Within this range, silver particles can fully contact and connect, forming a uniform and stable conductive network, thereby achieving optimal conductivity performance.
In addition to curing time, curing temperature is also an important factor affecting conductivity. The design of YB6016 low-temperature conductive silver paste from Yanbo brand enables it to cure at lower temperatures, typically around 150 ° C. Appropriate curing temperature can accelerate the contact and connection of silver particles, promoting the formation of conductive networks. However, excessively high curing temperatures may lead to excessive aggregation of silver particles and excessive decomposition of organic components, which in turn reduces conductivity.
In practical applications, in order to ensureResearch Platinum Brand YB6016 Low Temperature Conductive Silver AdhesiveAttention should be paid to the following points regarding the conductivity of:
Strictly control the curing time and temperature: According to the technical parameters provided by Advanced Institute (Shenzhen) Technology Co., Ltd., strictly control the curing time and temperature to ensure that the silver adhesive is cured under optimal conditions.
Avoid multiple curing: Multiple curing may cause changes in the internal structure of the silver paste, affecting its conductivity. Therefore, in practical operation, multiple curing should be avoided as much as possible.
Keep the work environment clean: Dust and impurities in the work environment may affect the curing effect of silver paste, thereby affecting its conductivity. Therefore, maintaining a clean working environment is very important.
In summary, the curing time has a significant impact on the conductivity of low-temperature conductive silver paste. By controlling the curing time and temperature reasonably, it is possible to ensure that the silver paste is cured under optimal conditions, thereby achieving the best electrical conductivity. Advanced Institute (Shenzhen) Technology Co., Ltd., with its professional technology and rich experience, provides users with high-quality low-temperature conductive silver paste to help the development of the electronics industry.
The above data is for reference only, and specific performance may vary due to production processes and product specifications.
Advanced Institute (Shenzhen) Technology Co., Ltd, © two thousand and twenty-onewww.avanzado.cn. All rights reservedGuangdong ICP No. 2021051947-1 © two thousand and twenty-onewww.xianjinyuan.cn. All rights reservedGuangdong ICP No. 2021051947-2