Advanced Institute Technology YB-5012 is a negativePhotosensitive conductive silver pasteHas excellent printability and conductivity on various substrates; It also has good fluidity and leveling performance, and the printing thickness can be controlled between 4-6um, which can meet the fine line etching of 30um. It is mainly used in the production of capacitive touch screens, flat panel displays, RFID and other high-precision circuits.
Product Features
Photosensitive silver pasteNegative photosensitive conductive silver paste
Negative Tone Photodefinable Conductive Silver Paste
Fine etching processing of photosensitive silver paste (line width/line spacing L/S, L: 30/30um)
Fine Etching Performance (line width/Space,L:30μm,S:30μm)
Excellent electrical performance (volume resistivity<1.0 × 10-4 Ω. cm)
Excellent Electrical Performance (Volume Resistance <1.0×10-4Ω.cm)
performance parameter
Test project testing tool/standard SILCON PD-716L
Viscosity RION VT-04F, 2nd rotor@ 25℃250±50dPa.s
Curing conditions: oven curing at 140 ℃ for 60 minutes
Volume resistivity four probe square resistance meter KDY-1 ≤ 1 × 10-4 Ω• cm
Adhesion hundred grid test, 3M600 tape 5B
Surface hardness Mitsubishi pencil ≥ 2H Note: The above data is the result of SILMAC laboratory testing and may vary slightly due to different testing conditions and environments. It is for reference only.
Testing Parameters
Project content parameters
Printing machine type: semi-automatic/fully automatic screen printing machine
Scraper angle 70~80 °
Scraper hardness 75~80
Printing screen mesh size 500 mesh steel mesh/420 mesh polyester mesh
Photographic adhesive thickness 5-7 μ m
Screen tension 23~28N
Stretch the net at an angle of 22.5 degrees
Dry condition oven at 80 ℃ for 10 minutes
Exposure UV exposure machine 300~500mJ/ cm2@365nm
Developing solution 0.2wt.% Na2CO3(30℃)
Developing pressure 0.2MPa
Development time 30-50S
Storage and usage methods
1. Avoid light exposure (0-5 ℃), with a validity period of 6 months from the date of production.
2. After refrigeration, it needs to be left for 2-3 hours to recover to room temperature, and thoroughly stirred for 15 minutes before printing.
3. The viscosity of the product has been adjusted, and it is not recommended to use diluents. If there are special requirements, it is recommended to use the matching diluent.
Advanced Institute (Shenzhen) Technology Co., Ltd, © two thousand and twenty-onewww.avanzado.cn. All rights reservedGuangdong ICP No. 2021051947-1 © two thousand and twenty-onewww.xianjinyuan.cn. All rights reservedGuangdong ICP No. 2021051947-2